25 de junio Filtro de espuma cerámica de aluminio Podgorica
Filtro de espuma cerámica de aluminio Podgorica is installed in the CFF box machine to filter the impurities in the aluminum alloy liquid to meet the high value-added, high-tech performance aviation, transportation and other aluminum alloy precision casting production.
The advantages of Ceramic Foam Filter Aluminium Podgorica include
1. Reduce the gas and inclusions contained in the casting, reduce the turbulence of the molten metal during filling, and reduce the surface defects of the casting.
2. Significantly reduce the rejection rate of castings, improve the compression and sealing performance of the castings, and increase the elongation and tensile strength of the castings.
3. Improve the surface finish of the casting, improve the fluidity of the molten metal, and improve the filling capacity of the melt.
4. Reduce processing time and tool wear, and improve the surface quality of castings.
Aluminium Podgorica chooses different filtering precisions during the use of ceramic foam filter
1. Selección de barras de aleación de aluminio: 10-30 ppi
2. Opciones de fundición a largo plazo: 30-50 ppi
3. Selección de perfiles o chapas de aluminio de alta calidad: 40 o 50 ppp
4. Opciones de colada continua y laminación de papel de aluminio: > 50 ppi
At present, there are various methods to remove these harmful substances and purify the aluminum melt.
According to different methods, it can be divided into two categories: in-furnace processing and continuous processing outside the furnace (that is, online processing).
According to the role, it can be divided into two categories: mainly degassing or deslagging. Ceramic casting filter manufacturer (www.adtechamm.com) introduced the use of foam ceramic filter plates to continuously filter aluminum melt. In addition to continuous treatment, the main purification operation is slag removal.
How to use ceramic filter plate
1. Clean the filter box
2. Coloca con cuidado la placa filtrante en la caja del filtro y presiona con la mano la junta de estanqueidad que rodea la placa filtrante para evitar que se escape el aluminio fundido.
3. Preheat the filter box and the filter plate uniformly to make them close to the casting aluminum liquid temperature.
4. Pay attention to the changes of the aluminum hydraulic head during casting. The normal initial pressure head is 75-150mm. When the molten aluminum starts to pass, the pressure head will drop below 25mm. Then the pressure head will slowly increase.
5. After filtering, take out the filter plate in time and clean the filter Box.















No Comments